I was thinking maybe 80lb or 60lb brockway or Mowhawk (if there are
better options, let me know). Portrait orientation.
Still-Leaf sounds very promising, I would like to know more
information, definitely.
----- Original Message ----
[Please respond to Book_Arts-L@xxxxxxxxxxxxxxxx]
From: George Baker [mailto:geembee@xxxxxxxxxxxxxx]
Sent: Tuesday, November 04, 2008 12:41 PM
Subject: Conductors score
You did not mention the type or weight, (caliper,) of the paper or
the
orientation of the text. I assume the page attachment would be at
one 11
inch edge. If the weight of the paper is sufficient, say 150 to
200 gsm you
might consider a stiff-leaf binding. Stiff leafs open flat. if
this appeals
to you I can go into more detail. George M, Baker