Marguerite,
I know that the Rare Book and Manuscripts Library provides regular Purell
for its patrons to use before handling materials. As far as I know, as long
as the Purell is completely dry before touching any materials, the product
does not leave any residue. Good luck!
Heather Marie Kosur
Milner Library
Illinois State University
-----Original Message-----
From: Book_Arts-L [mailto:BOOK_ARTS-L@xxxxxxxxxxxxxxxx] On Behalf Of
Marguerite Radhakrishnan
Sent: Thursday, January 08, 2009 9:14 AM
To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
Subject: Re: [BKARTS] Question re "liquid gloves"
Our collection manager has a question along those lines, which I've
asked elsewhere but seems to be appropriate here as well: is there any
sort of alcohol wipe that would remove grime/oils, yet not leave a
residue? (and be easier than "please go wash your hands, but we can't
be sure you have, since we're not in the bathroom with you, and anyhow
the soap we're provided with and have no control over is 'with lotion'
so we lose out either way.")
--Marguerite Radhakrishnan
On Thu, Jan 8, 2009 at 8:42 AM, Jet Foncannon <bolu.bolu@xxxxxxxxxxx> wrote:
> The fact is, one can't work with books and use any kind of hand
emollient
> or softener. (Many rare book collections realize this. The Rosenbach
> library, in Philadelphia, requires all visitors to wash their hands before
> viewing the collection.)
***********************************************
Annual Arnold Grummer Press sale now online at
<http://www.philobiblon.com/suppliers.shtml#Press_Sale>
Please note that attachments to listserv messages are not permitted,
and are automatically removed by the listserver.
For all your subscription questions, go to the Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information.
***********************************************
***********************************************
Annual Arnold Grummer Press sale now online at
<http://www.philobiblon.com/suppliers.shtml#Press_Sale>
Please note that attachments to listserv messages are not permitted,
and are automatically removed by the listserver.
For all your subscription questions, go to the Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information.
***********************************************