I am surprised to hear about using mat board.  While it is certainly a good
material in terms of composition (at least certain brands which are 100%
cotton) it is a very low density material.  I also know that is made by
laminating multiple layers together, hence how the thickness are represented
in the framing industry (2ply, 4ply, 8ply, etc), and can delaminate.  

The density is however the biggest concern and am surprised that you would
find the corners to be more durable than that of Davey board.  The
application of mat board is that of making window mats for framing so
density and durability are not paramount characteristics.  

I can certainly see people using it and recommending it since it is readily
available in local art stores, and maybe that is why it is mentioned.  Mat
Board is also a much more expensive material.  The Eterno Board we sell is
great as well, but a much different price point than Davey as well.

Regards,
Aaron Salik

Talas
330 Morgan Ave
Brooklyn, NY 11211
212-219-0770 Phone
212-219-0735 Fax
http://talasonline.com

                                    
             ***********************************************
                                    
       NOW ONLINE, Volume 5, No. 2, Spring 2009 of The Bonefolder
       <http://www.philobiblon.com/bonefolder/vol5no2contents.htm>
                                    
  Please note that attachments to listserv messages are not permitted,
            and are automatically removed by the listserver.
                                    
For all your subscription questions, go to the Book_Arts-L FAQ and Archive.
         See <http://www.philobiblon.com> for full information.
                                    
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]