    The joint tacketing technique was devised by the conservation department
    at Trinity College, Dublin and is illustrated in a pamphlet called
    'Preserving our Printed Heritage' published by Trinity College. ISBN
    0904720187.

Alison Hamilton
Conservator
University of London Library
Senate House, Malet Street
London WC1E 7HU

                                  ***