Rubber cement

From: Paul Messier <pmessier>
Date: Tuesday, February 7, 1995
While rubber cement solvent is available, this product works only on new
rubber cement.  As the cement ages its solubility parameters change. Its
also worth noting that some photographs (collodion papers, among others)
can be very seriously harmed by direct contact with many organic
solvents.