One of our students is working on some Chinese miniature paintings on
so-called "pith paper", which is also referred to as "Tsuso paper" or
"rice paper". The paintings are very fragile and brittle and need to be
restored in some way.

I would like to hear if anyone has some experience or practical
information about the conservation and restoration of pith paper.
Furthermore, do you know where we can buy new pith paper. Thanks,

Ingelise Nielsen
School of Conservation
Esplanaden 34
DK-1263 Copenhagen K, Denmark
Fax: +45 3332 0801

                                  ***
                  Conservation DistList Instance 8:63
                 Distributed: Sunday, February 12, 1995
                        Message Id: cdl-8-63-010
                                  ***
Received on Saturday, 11 February, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/0130.html
Timestamp: Wednesday, 12-Jun-2013 22:31:33 PDT
Retrieved: Wednesday, 13-Nov-2019 22:11:05 GMT