In regards to archival photocopies, the people at the National Archives
have developed a simple peel test to determine if the toner is properly
fused onto the paper.  "Archival Copies of Thermofax, Verifax and Other
Unstable Records" by Norvell M.M. Jones, National Archives Technical
Information Paper No. 5, 1990.