What do people use to adhere Plastazote (which as I understand it is a
cellular polyethylene foam) to wood?

I would usually HMG Cellulose Nitrate or HMG B72 but the laboratory
people at HMG tell me that they suspect HMG adhesives will react with
the cellular polyethylene foam.

Mark Vine