Laser printing is as stable as photocopying as long as it *is* from a
laser printer--if they were produced on a bubble-jet printer they are
highly water soluble.

There is an article which may help: "The Conservation of faxes and
colour photocopies with special reference to David Hockney's 'Home made
prints'", by Heather Norville-Day, in Modern Works Modern problems,
Institute of Paper Conservation Conference, 1994