Now that I know what's in 3M #4475 I do not even have any interest in
trying it.  And yes, I do use B-72 in a great number of treatments, and
it does have good reasons for "defense" and justification.  However, I
do agree with Geoffrey Brown that it does not do all things equally
well, and "discretion is the better part of...conservation". Still, I am
very pleased with its workability and reversibility, as well as other
adhesive properties.  It is compatible with cellulose nitrate adhesives,
and by modifying the solvents and solids ratio, it may be suitable for
Mark Vine's hair problem.  I recommend testing on a mock-up, and suggest
that the acetone may be less of a problem for the re-treatment aspect
than applying an adhesive with MEK (though I doubt it is the only
solvent in 4475).

                                  ***
                  Conservation DistList Instance 8:82
                   Distributed: Sunday, April 9, 1995
                        Message Id: cdl-8-82-003
                                  ***
Received on Tuesday, 4 April, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/0369.html
Timestamp: Wednesday, 12-Jun-2013 22:31:33 PDT
Retrieved: Wednesday, 18-Sep-2019 07:36:41 GMT