Subject: Labeling encapsulated materials
In response to Sherry Byrne's problem of labeling encapsulated maps: By far the best solution, assuming you are using mylar, is to encapsulate the label into the mylar (outside the space housing the object) using an ultrasonic welder. If you do not have a ultrasonic welder, I would recommend housing the mylar-encapsulated maps inside slightly larger folders, preferably in 40 or 60 pt. lignin-free folders. The folders themselves can be lightly labeled with #3 pencils. George Leake Harry Ransom Center Univ of Texas at Austin *** Conservation DistList Instance 8:89 Distributed: Sunday, May 7, 1995 Message Id: cdl-8-89-008 ***Received on Thursday, 4 May, 1995