Daguerreotypes

From: Mark Clarke <markey>
Date: Tuesday, July 18, 1995
Don't touch the image surface.

Then, look at "The Conservation of Photographs", 1985, Eastman Kodak
Company (my copy came from from Archetype Books, London, +44 171 387
9651).

As this explains, pps. 132 ff, liquid or abrasive treatments have
all been found to cause damage, and often revert. Kodak advise
preservation "until harmless cleaning methods become known".

Reseal in a 19th century manner using a new stable coverglass and
mat. Tape edges & store. (40 % RH, 70 deg F).  Good luck,

Mark Clarke
+44 171 277 1633

                                  ***
                  Conservation DistList Instance 9:11
                 Distributed: Wednesday, July 19, 1995
                        Message Id: cdl-9-11-004
                                  ***
Received on Tuesday, 18 July, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/0647.html
Timestamp: Wednesday, 12-Jun-2013 22:31:34 PDT
Retrieved: Saturday, 14-Dec-2019 00:25:36 GMT