I am looking for information which will help me determine the next
course of treatment for an unfixed, pastel drawing with complex
tears, stains and distortions on thin, degraded, wood-pulp paper
(like butchers paper).  Has anyone had any good/bad experiences
humidifying, float or wet blotting paper washing and lining such
awkward items using suction table or other methods, or know of any
published articles\case histories? I would greatly appreciate
hearing from you,

Lynda Black
Paper Conservator
Commercial Conservation Section
State Library of Queensland
Brisbane, Australia

                                  ***
                  Conservation DistList Instance 9:18
                Distributed: Wednesday, August 23, 1995
                        Message Id: cdl-9-18-003
                                  ***
Received on Monday, 21 August, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/0752.html
Timestamp: Wednesday, 12-Jun-2013 22:31:34 PDT
Retrieved: Monday, 23-Sep-2019 00:47:58 GMT