>Carol Brown's posting requested information on materials for
>conserving Whale Bone.
>
>Might HMG Cellulose Acetate adhesive be used in this context, it has

I do not believe HMG makes a cellulose "acetate" adhesive. The "old"
HMG (in the blue tube) is a cellulose *nitrate*; the "new" HMG (in
the purple tube) is Acryloid (Paraloid) B-72.

Stephen Koob
Department of Conservation and Scientific Research
Freer Gallery of Art
Smithsonian Institution
Washington DC 20560
202-357-4880 x276

                                  ***
                  Conservation DistList Instance 9:24
                Distributed: Saturday, September 9, 1995
                        Message Id: cdl-9-24-005
                                  ***
Received on Thursday, 7 September, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/0809.html
Timestamp: Wednesday, 12-Jun-2013 22:31:34 PDT
Retrieved: Saturday, 07-Dec-2019 14:33:42 GMT