Does anyone have any suggestions for removing red permanent marker
from an acrylic painting?  We have tried various solvents including
mineral spirit, toluene, alcohols and acetone alone and in
combination.  Thus far, everything that dissolves the marker also
affects the acrylic paint.  We made up test panels to try and fade
the marker under intense light and we have tried a dry cleaning
method with eraser.  So far nothing seems to work.

Patricia Smithen

                                  ***
                  Conservation DistList Instance 9:25
               Distributed: Thursday, September 14, 1995
                        Message Id: cdl-9-25-001
                                  ***
Received on Monday, 11 September, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/0816.html
Timestamp: Wednesday, 12-Jun-2013 22:31:34 PDT
Retrieved: Wednesday, 13-Nov-2019 02:05:07 GMT