I've found that a Berol Prismacolor Non-photo blue 919 or a Berol
China Marker brite blue 167T will write on RC paper, does not easily
smear, and is reversible. The Prismacolor Non-photo blue can be
erased with a common eraser and the china marker can be rubbed clean
with a cotton cloth.

Peter J. Roberts
Audio-Visual Archivist
Georgia State University

                                  ***
                  Conservation DistList Instance 9:29
                Distributed: Tuesday, September 26, 1995
                        Message Id: cdl-9-29-003
                                  ***
Received on Monday, 25 September, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/0876.html
Timestamp: Wednesday, 12-Jun-2013 22:31:34 PDT
Retrieved: Sunday, 08-Dec-2019 21:29:16 GMT