Maria Mavrommati <maria [at] spark__net__gr> writes

>The reinstallation of mosaics is our next step. The problem we face
>is to fill those 3 meters with the proper and best stuff available.

Might Primal AC33 may be a suitable acrylic emulsion for mosaic
restoration? It has I am informed been used for the consolidation
and repair of crumbling sandstone, masonry and mortar.

Comparing Primal WS24 to Primal AC33:

    Solid content    36%               46-47%
    pH               7                 9.4 to 9.9

AC33 has excellent freeze-thaw stability, a wide tolerance to
pigments and a high viscosity.

In the United Kingdom as a result of requests from conservators we
have recently taken the product on offering it in litre units as we
do Primal WS24.

Mark Vine
Conservation Resources, England

                                  ***
                  Conservation DistList Instance 9:41
                Distributed: Saturday, November 11, 1995
                        Message Id: cdl-9-41-004
                                  ***
Received on Tuesday, 7 November, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/1059.html
Timestamp: Wednesday, 12-Jun-2013 22:31:34 PDT
Retrieved: Sunday, 22-Sep-2019 15:01:11 GMT