We currently use an ELSEC UV TYPE 762.  As we have had it for a
while, and as technology marches ever forward, we would like to know
if anyone has any advice on upgrading.  Is it the case that the
cognoscenti would say "Oh, everyone now uses the Supergalactic
Whizbang Whatsis"?

Henry Grunder

                                  ***
                  Conservation DistList Instance 9:45
                 Distributed: Friday, December 1, 1995
                        Message Id: cdl-9-45-015
                                  ***
Received on Monday, 27 November, 1995










[Search all CoOL documents]

FAIC
CoOL and DistList SURVEY

We need your help. FAIC seeks to improve CoOL and the DistList, and increase their value to the conservation field and beyond. In an effort to do so, we have put together a short, voluntary survey of DistList subscribers and other users of the CoOL website and its various resources. Please help us develop these invaluable resources by taking a few minutes to complete the survey


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/1118.html
Timestamp: Wednesday, 03-Mar-2010 10:49:22 PST
Retrieved: Sunday, 14-Mar-2010 20:27:30 GMT