Can acetone be safely used to remove grease build-up from the
surface of a globe? The globe is made of paper strips and evidently,
a glossy surface remains after a test patch was wiped down with a
cotton pad dampened with acetone.  The pad also picked up some ink.
Water solutions saturated the edges of the paper strips.

The man posting the query estimates the globe to be 30 to 40 years
old. Also, what sort of finish should be applied to protect the
globe after the grease has been removed?

Thanks for any suggestions.

Sue Stoebner

                                  ***
                  Conservation DistList Instance 9:48
                 Distributed: Monday, December 11, 1995
                        Message Id: cdl-9-48-008
                                  ***
Received on Wednesday, 6 December, 1995










[Search all CoOL documents]

FAIC
CoOL and DistList SURVEY

We need your help. FAIC seeks to improve CoOL and the DistList, and increase their value to the conservation field and beyond. In an effort to do so, we have put together a short, voluntary survey of DistList subscribers and other users of the CoOL website and its various resources. Please help us develop these invaluable resources by taking a few minutes to complete the survey


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/1156.html
Timestamp: Wednesday, 03-Mar-2010 10:49:22 PST
Retrieved: Sunday, 21-Mar-2010 00:30:46 GMT