>Has anyone who has been using Kapco covers for a number of years
>have any evidence that the covers contribute to the separation of
>the cover from the textblock when the attachment is hot melt glue?

With regard to hot glue bindings failing after application of Kapco
covers, those glue bindings, I am advised, fail because of the lack
of air circulation even when Mylar tape is applied to the spine
area.  We do this as a preventive measure (Mylar) and use quite a
bit of Kapco EZ bind tape in our mendery, though we do not use Kapco
covers.  Demco representatives are the source of this information,
given in a mends presentation.

Elaine Schiller
Senior Collection Maintenance Assistant
Timberland Regional Library
415 Airdustrial Way SW
Olympia, WA  98501-5799
360-943-5001
Fax: 360-586-6838

                                  ***
                  Conservation DistList Instance 9:50
                Distributed: Saturday, December 23, 1995
                        Message Id: cdl-9-50-015
                                  ***
Received on Monday, 18 December, 1995

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1995/1198.html
Timestamp: Wednesday, 12-Jun-2013 22:31:34 PDT
Retrieved: Tuesday, 19-Nov-2019 02:17:12 GMT