Subject: Tape

Tape

From: Gary Frost <dryfrio>
Date: Saturday, December 13, 1997
Rose Sheridan <rsheridan [at] little-dixie__lib__mo__us> writes

>After a little persuasion, I did get the staff to switch from
>regular adhesive tape to the removable tape.  It's still not good,
>but at least it's less damaging to the materials.  My problem is
>that after using the tape for a couple of months, people are
>complaining that it doesn't stick very well and they want to go back
>to the old way of using regular sticky tape to attach notes to
>books.  The topic will surely come up at our staff meeting in
>January, and will I need to be prepared to defend my stance.

Perhaps you should shift the discussion to where the taped notes are
placed. The back pastedown or its free flyleaf? There is also the
option of tipping in a sacrificial blank flyleaf for the tape
mountings.

As for page mending, the tissue based repair tapes are less damaging,
though not from a legibility standpoint. In a broad consideration of
their damage potential all tapes are just too wide for page mending.
For page mending, scissor cut the tape lengthwise into short, narrow
strips.

Tapes should not be used on books published prior to their
invention. This is a weird rule that appeals to librarians.

Gary Frost

                                  ***
                  Conservation DistList Instance 11:54
               Distributed: Wednesday, December 17, 1997
                       Message Id: cdl-11-54-010
                                  ***
Received on Saturday, 13 December, 1997










[Search all CoOL documents]

FAIC
CoOL and DistList SURVEY

We need your help. FAIC seeks to improve CoOL and the DistList, and increase their value to the conservation field and beyond. In an effort to do so, we have put together a short, voluntary survey of DistList subscribers and other users of the CoOL website and its various resources. Please help us develop these invaluable resources by taking a few minutes to complete the survey


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1997/1581.html
Timestamp: Wednesday, 03-Mar-2010 10:49:24 PST
Retrieved: Thursday, 18-Mar-2010 20:27:48 GMT