In response to Dee Stubbs' inquiry about repairing a Chinese
cloisonne artifact, I suggest using Hxtal in a composition with dry
pigment, marble flour and fumed silica.  In working with chinese
objects, I have found that marble flour gives the composition
appropriate opacity without making the color seem dead.  The fumed
silica should give you a matte finish.  If you need to dull it more,
a light application of denatured alcohol should do the trick.

Dale Freedman
(private practice)
Newton, MA
617-243-3003

                                  ***
                  Conservation DistList Instance 12:20
                Distributed: Wednesday, August 26, 1998
                       Message Id: cdl-12-20-003
                                  ***
Received on Thursday, 13 August, 1998

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1998/0987.html
Timestamp: Wednesday, 05-Oct-2011 15:20:15 PDT
Retrieved: Monday, 17-Feb-2020 10:21:42 GMT