Another source of silver sheet is

    Goodfellow Corporation
    800 Lancaster Avenue
    Berwyn, PA 19312-1780
    1-800-821-2870
    <URL:http://www.goodfellow.com/>

They supply various thicknesses of 99.95+% silver foil.  Their
AG000350 is 0.1mm thick.  1 piece, 50 X 50 mm, costs $141.00, but if
you order 50, the price is $412.  That's $20.60/sheet, which beats
Aaron Alpha.

Incidentally, I don't think that the sheet thickness is going to
matter much in these tests, but the purity may.  I liked Will
Jeffers's questions and would be interested to hear more about the
purity issue.

    **** Moderator's comments: Thanks also to Regis Bertholon
    <bertholon7 [at] aol__com> who provided similar information

Tom Chase
Chase Art Services
Chevy Chase, MD.

                                  ***
                  Conservation DistList Instance 12:35
                 Distributed: Thursday, October 8, 1998
                       Message Id: cdl-12-35-006
                                  ***
Received on Sunday, 4 October, 1998

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1998/1189.html
Timestamp: Wednesday, 05-Oct-2011 15:20:15 PDT
Retrieved: Friday, 28-Feb-2020 22:05:18 GMT