>We need to clean a ceiling painted with tempera that is actually
>covered with a thick lay of soot.

I have with good results used an acid-free rubber pad called
"Wishab", obtained in three grade: soft--hard--extra-hard (I prefer
the hard quality) from Germany in a box with 30 pads, which make it
possible for you to share them with your colleagues:

    Akachemie, Zeppelinstr. 10-12
    Postfach 1152
    D-7315 Weilheim

This rubber pad can be used for dry-cleaning on all kind of solid
materials such as paper, leather, parchment etc.

    **** Moderator's comments: Thanks also to Olaf Pung
    who also mentioned this product

Soren Ibsen
Book- and paperrestorer
Norwegian University of Science and Technology
University Library of Trondheim
Gunnerus Library
N-7034  Trondheim
+47 7359 2132
Fax: +47 7359 2100

                                  ***
                  Conservation DistList Instance 12:46
                 Distributed: Monday, November 23, 1998
                       Message Id: cdl-12-46-007
                                  ***
Received on Thursday, 19 November, 1998

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1998/1408.html
Timestamp: Wednesday, 05-Oct-2011 15:20:15 PDT
Retrieved: Saturday, 29-Feb-2020 00:38:00 GMT