Robert J. Milevski <milevski [at] phoenix__princeton__edu> writes

>I have a research project on the horizon, part of which involves
>binders cover stamping dies.  I want to make sharp dark impressions
>of these dies for scanning into a computer.  I want to do this, if
>possible, without heating them up individually in a hot stamping
>press.

Would it be possible to photograph the dies in black and white under
slightly raking light and then transfer the image to a scanner?
Kodak might be able to suggest which film and developer would give
the most contrast.

Karen L. Pavelka
pavelka [at] mail__utexas__edu
Senior Lecturer, Preservation and Conservation Studies
Graduate School of Library and Information Science
SZB 564/D7000, University of Texas at Austin
Austin, Texas 78712-1276
512-471-8286
Fax: 512-471-8285

                                  ***
                  Conservation DistList Instance 12:48
                 Distributed: Monday, November 30, 1998
                       Message Id: cdl-12-48-011
                                  ***
Received on Monday, 30 November, 1998

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/1998/1448.html
Timestamp: Wednesday, 05-Oct-2011 15:20:15 PDT
Retrieved: Friday, 21-Feb-2020 13:29:36 GMT