Could someone direct me to a supplier of Desogen (Ciba-Geigy) or Dimanin (Bayer), possibly in Canada or N.A. As you well know both are quaternary ammonium salts used in the AB 57 solution to clean and disinfect mural paintings. Ciba-Geigy (now Novartis) seems to be unaware of the product they used to produce and Bayer doesn't answer my e-mails. Are you aware of a possible equivalent substitute? Pierlucio Pellissier in Montreal *** Conservation DistList Instance 15:78 Distributed: Monday, May 20, 2002 Message Id: cdl-15-78-009 ***Received on Fri May 17 2002 - 00:00:00 PDT