Concerning lightfast felt-tip pens to be used on plastics like
polyethylene, many of us might regret that Staedtler Pancolor 303 is
no longer available. While Pancolor 303 used lightfast pigments, the
follow-up Staedtler Lumocolor permanent is using dyes. Lumocolor
permanent is still called "lightfast" but according to the
manufacturer it is much less lightfast than the predecessor,
Pancolor 303. Does anybody know a good replacement for Pancolor 303
(for example for marking plastics)?

Christoph Waller
Long Life for Art
Im Bueckle 4
D- 79299 Gottenheim
+49 7665 94 03 90
Fax: +49 7665 94 03 91


                                  ***
                  Conservation DistList Instance 16:74
                   Distributed: Tuesday, May 27, 2003
                       Message Id: cdl-16-74-014
                                  ***
Received on Sunday, 25 May, 2003

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2003/0700.html
Timestamp: Thursday, 26-Jan-2012 15:56:53 PST
Retrieved: Wednesday, 16-Oct-2019 22:10:15 GMT