Subject: Nitrile gloves

Nitrile gloves

From: Ellen Pearlstein <epearlstein>
Date: Thursday, June 26, 2003
Will Jeffers <wjeffers [at] mfa__org> writes

>After hearing about problems with silver tarnishing after it had
>been handled with a specific brand of powder free nitrile gloves, I
>ran some quick accelerated corrosion tests on several brands of
>nitrile gloves.

Could you identify the brands of the gloves you tested?  Thanks.


                                  ***