I just received a shipment of 1/2 x 3 inch Brainerd mending plates
from United Manufacturers Supply, which appear to be real brass. The
last bunch we got from them were nearly impossible to bend without
snapping, so these are an improvement.  I am not sure about their
longer ones (I believe they only go to 4 inches).  You can check
<URL:http://www.unitedmfrs.com/> and find out.

In addition, I am in the process of seeking a shop to manufacture
these to meet our specifications.  As I learn more, I'll post it
here.

Jim Williams
Project Coordinator
Intermuseum Conservation Association
2915 Detroit Ave
Cleveland, OH  44113
216-658-8700


                                  ***
                  Conservation DistList Instance 17:34
                Distributed: Thursday, October 16, 2003
                       Message Id: cdl-17-34-010
                                  ***
Received on Thursday, 9 October, 2003

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2003/1338.html
Timestamp: Thursday, 26-Jan-2012 15:56:53 PST
Retrieved: Thursday, 18-Jul-2019 05:05:57 GMT