Subject: Adhesives for baleen

Adhesives for baleen

From: Jim Wortman <jim>
Date: Monday, January 8, 2007
I am evaluating the potential restoration of a late 1960's Alaskan
Inuit built ship model, 2 feet long.  The hull and sails are made of
male and female baleen respectively. The hull is canoe shaped and
sewn together along the keel and up the bow and stern. During a
poorly packed shipping attempt, a 4 inch section of the hull broke
off near the bow as well as receiving a 6 inch stress fracture on
its other side.

Does anyone have any experience with adhesives compatible with
baleen?  It is now quite brittle and misshapened.  Any suggestions
concerning the stress fracture? Would heat application make it
malleable enough to repair?

Jim Wortman
Model Shipwright
Talbot Ship and Rail
PO Box 460
St. Michaels, MD 21663
410-745.6268


                                  ***
                  Conservation DistList Instance 20:35
                 Distributed: Monday, January 15, 2007
                       Message Id: cdl-20-35-014
                                  ***
Received on Monday, 8 January, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/0041.html
Timestamp: Thursday, 13-Jun-2013 08:14:24 PDT
Retrieved: Wednesday, 22-May-2019 17:12:13 GMT