Benzotriazol

From: Howard B. Wellman <hwellman>
Date: Friday, May 18, 2007
Sabine Brechbuhl <sabine.brechbuehl [at] erz__be__ch> writes

>Can a bath of benzotriazol, BTA 3% in ethanol during 24 hours
>(according to D. A. Scott, Copper and Bronze in Art), penetrate
>enough and if so, is this stabilisation effective even on a
>consolidated object?

I do not expect that the BTA will penetrate effectively through the
B-72 consolidant to bond to the copper alloy substrate.

Ideally, you should remove the B72, then apply the BTA by immersion
under vacuum, then reconsolidate as necessary.

Howard Wellman
Maryland Archaeological Conservation Laboratory
410-586-8577


                                  ***
                  Conservation DistList Instance 21:7
                   Distributed: Monday, May 28, 2007
                        Message Id: cdl-21-7-005
                                  ***
Received on Friday, 18 May, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/0584.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Saturday, 07-Dec-2019 09:24:24 GMT