Date: Tuesday, May 15, 2007
I am working on a bronze object that has been consolidated with
Paraloid B-72 three years ago. This is my Diploma project for
Object conservation at the Fachhochschule fuer Technik und
Wirtschaft in Berlin. I am asking myself now, if someone has
experienced that Paraloid B-72 is not soluble after a certain
period of time. Although Paraloid does hardly change with time, it
might get irreversible after 10-20 years. Has someone tried to
dissolve Paraloid after more than 10 years?

Lena Tietjen
FHTW (Fachhochschule fuer Technik und Wirtschaft) Berlin


                                  ***
                  Conservation DistList Instance 21:7
                   Distributed: Monday, May 28, 2007
                        Message Id: cdl-21-7-024
                                  ***
Received on Tuesday, 15 May, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/0602.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Wednesday, 22-May-2019 17:29:11 GMT