Subject: Ultrasuede

Ultrasuede

From: Paul Himmelstein <aandh>
Date: Wednesday, May 30, 2007
I have been asked about the possibility of using black "ultrasuede"
as a covering fabric inside an exhibition case for books.  Has
anyone looked at the off gassing potential of this material?  I
realize that synthetic,imitation suede is made by a number of
manufacturers  I have no idea who makes this particular one.  I seem
to remember someone saying that the basic material is fairly stable,
but that may have been cocktail talk at an AIC meeting!

    **** Moderator's comments: Toray Ultrasuede (America), Inc. See
    <URL:http://www.ultrasuede.com/about/faq.html>

Paul Himmelstein
Appelbaum and Himmelstein
444 Central Park West
New York, NY  10025
212-666-4630


                                  ***
                  Conservation DistList Instance 21:9
                   Distributed: Friday, June 8, 2007
                        Message Id: cdl-21-9-035
                                  ***
Received on Wednesday, 30 May, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/0662.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Saturday, 25-May-2019 11:24:15 GMT