This is from Myra L. O'Canna <mlocann [at] sandia__gov>, who is not on the
list:

  I'm helping a church assemble a time capsule. They want to use two
  fiberglass containers to hold their items as those containers are
  used to hold various church implements.  Do you think those would
  be acceptable containers for a period of 50 years?

  Myra O'Canna