Conservation DistList Archives [Date] [Subject] [Author] [SEARCH]

Subject: Latex dinosaur model

Latex dinosaur model

From: Ed Jarzembowski <edjarzembowski>
Date: Friday, September 21, 2007
    **** Moderator's comments: This query comes from a person who is
    not on the DistList and will not see any responses that are
    posted here.  Please respond directly to sender, Ed Jarzembowski
    <edjarzembowski [at] maidstone__gov__uk>, and if of general interest
    post it here as well
Our
popular old dinosaur model (latex skin) is beginning to liquefy at
the joints. Is there anything we can do to stop this?

Ed Jarzembowski (Prof Dr)
Keeper of Natural History


                                  ***
                  Conservation DistList Instance 21:24
               Distributed: Saturday, September 29, 2007
                       Message Id: cdl-21-24-028
                                  ***