This enquiry is posted on behalf of a colleague who owns a
home-stored collection of some 300-400 comics, unopened in their
original "plastic" wrappers.

He is seeking advice about their best means of long-term storage and
preservation, in home conditions. He believes that some have
monetary value, but has limited funds for buying specialist storage
materials.

The comics date from the 1960s-1990s. All are in their original
"plastic" wrappers, unopened and without apparent ventilation holes
in the wrappers. They are stored piled into sealed cardboard boxes.

Issues seem to include: degradation of the plastic wrappers;
possible reactions between the paper comics and plastic wrappers;
ferrotyping of the print onto the plastic; differing microclimates
within individual wrapped comics, especially where plastic wrappers
may not be completely sealed; achieving best overall environmental
conditions.

He would appreciate advice as to an effective low-cost storage and
preservation solution, should that be possible!

Paul Sillitoe


                                  ***
                  Conservation DistList Instance 21:24
               Distributed: Saturday, September 29, 2007
                       Message Id: cdl-21-24-035
                                  ***
Received on Sunday, 23 September, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/1063.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Saturday, 20-Jul-2019 14:33:47 GMT