Martin O'Brien <martinjob [at] earthlink__net> writes

Zbynek Jonak <zjonak [at] yahoo__com> writes

>>We are treating several pieces of furniture at a private residence.
>>One of the pieces is a large Nakashima dining table which has
>>developed a dull, sticky finish. ...
>...
>Unless the wax fails to give you proper color saturation, I would
>not attempt to apply tung oil.  You might consider contacting the
>Nakashima Studio.  I believe they are still quite active in New
>Hope, PA

In my opinion, contacting the Nakashima Studio as Mr. O'Brien has
suggested would be an important step. If I remember correctly from a
Discovery TV learning production, his daughter and son are
continuing the business.

    George Nakashima Woodworker, S.A.
    1847 Aquetong Road
    New Hope, PA 18938
    215-862-2272
    Fax: 215-862-2103
    info [at] nakashimawoodworker__com

Perhaps there is catalogue number on the table whereas the precise
coating could be verified.  I would not recommend cleaning with
steel wool as you would most likely contaminate the surface with
particles of steel wool becoming embedded in the coating.  Again, as
Mr O'Brien stated, a cleaning, after solvent testing would be in
order.

Robert Klein
Roberts Antiques Restoration
Pensacola, Fl


                                  ***
                  Conservation DistList Instance 21:27
                Distributed: Saturday, October 20, 2007
                       Message Id: cdl-21-27-004
                                  ***
Received on Saturday, 6 October, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/1131.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Saturday, 20-Jul-2019 14:09:20 GMT