I am working on a project for the display and long-term storage of
linoleum printing plates (used for linocut prints) dating from the
early 1930s. I have been able to find general information on the
composition of linoleum but I am wondering if anyone has information
on the degradation of this material.

The linoleum is brown in colour and it is off-gassing with a strong
linseed oil type odour, which is characteristic of linoleum. We are
looking into possible scavengers, such as activated charcoal, to
incorporate into the case and storage designs. I am particularly
interested in any information about this off-gassing since they will
be on display in an enclosed case for 1 year.

Laura Cunningham, Intern
Conservation Lab
Art Gallery of Ontario
317 Dundas Street West,
Toronto, Ontario, Canada


                                  ***
                  Conservation DistList Instance 21:28
                 Distributed: Friday, October 26, 2007
                       Message Id: cdl-21-28-024
                                  ***
Received on Wednesday, 24 October, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/1188.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Tuesday, 22-Oct-2019 23:30:08 GMT