I am a second year conservation student and have received a very
badly deteriorated mammoth tooth to conserve. It is delaminating and
crumbling to the touch and is currently being supported by bandages
to prevent it breaking in two when it is handled. It will obviously
need consolidation and I am aware that immersion in a solution of
Paraloid (Acryloid) B72 would be effective, but I would like to know
if there are any techniques that others have used that have proved
successful?

Elizabeth Dunford
University of Lincoln
UK


                                  ***
                  Conservation DistList Instance 21:31
               Distributed: Wednesday, November 21, 2007
                       Message Id: cdl-21-31-020
                                  ***
Received on Monday, 5 November, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/1266.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Thursday, 21-Nov-2019 21:04:02 GMT