Silvia Oliveira Sequeira <s.o.sequeira [at] gmail__com> writes

>In the literature we have not found any information about the
>combination of starch paste with copper. We thought maybe it was
>some insecticide or fungicide compound added to this bio-susceptible
>glue, but there is nothing on this subject in the articles we have
>found. Does anyone know anything about this starch paste/copper
>combination?

There are references to fungicides added to starch paste in the
publication The conservation of books and documents by WH Langwell
1957, There are two substances mentioned that could be the cause of
the green colour: copper naphthenate or copper oxinate.

Mark Allen, Conservator
Flintshire Record Office


                                  ***
                  Conservation DistList Instance 21:36
               Distributed: Wednesday, December 19, 2007
                       Message Id: cdl-21-36-002
                                  ***
Received on Wednesday, 19 December, 2007

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2007/1397.html
Timestamp: Thursday, 13-Jun-2013 08:14:25 PDT
Retrieved: Tuesday, 23-Jul-2019 19:36:52 GMT