I am an intern at the Smithsonian National Museum of the American
Indian.  Recently, I have come across a strand of plastic-looking
beads that appear to have insect damage.  They are bright pink and
are molded on the string (not loose beads).  The bead necklaces are
on a Huron or Wyandot doll that was accessioned in 1930.  No other
information is known about its history.  RAMAN spectroscopy revealed
the beads are made of starch (confirmed by a positive potassium
iodide test).  XRF revealed higher levels of zinc, rubidium, and
potassium in the beads than in the fabric of the doll.  I am looking
to do more research on this material and this type of bead.  Does
anyone have experience with this type of material?

Ashley Jehle
Pre-program Conservation Intern
Smithsonian National Museum of the American Indian
Cultural Resources Center
Suitland, MD 20746
301-238-1423
Fax: 301-238-3201


                                  ***
                  Conservation DistList Instance 21:54
                  Distributed: Friday, April 11, 2008
                       Message Id: cdl-21-54-019
                                  ***
Received on Thursday, 3 April, 2008

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2008/0383.html
Timestamp: Saturday, 06-Feb-2016 11:35:23 PST
Retrieved: Thursday, 17-Oct-2019 11:19:57 GMT