Tom Riddolls <tomriddolls [at] hotmail__com> writes

>A client recently brought to me a life-size wax figure that is very
>dusty. ...

If you have access to a laser this cleans wax successfully.If not
try dry cleaning with Wishab or other molecular trap or a dense (not
sloppy) Laponite gel over Japanese tissue.

Jane Foley ACR
Sculpture and Objects
Litas Liparini Restoration Studio
823 Main St Evanston Il 60202
847-491-0110


                                  ***