David Cox

From: Rebecca Ellison <rebecca.ellison<-a>
Date: Friday, May 16, 2008
I am currently working on an oil painting by the English painter
David Cox (1793-1859). It appears to be on paper, which has been
stuck onto a larger wooden panel, apparently at a later date. I have
taken an x-ray, which indicates that the original paper support has
been prepared with a ground layer containing lead white. I am
interested to know if any research has been carried out into Cox's
oil painting techniques.

Rebecca Ellison ACR
Oil Paintings Conservator
National Museum Wales
Cathays Park
Cardiff CF10 3NP
+44 2920 573 225


                                  ***
                  Conservation DistList Instance 21:61
                  Distributed: Saturday, May 17, 2008
                       Message Id: cdl-21-61-025
                                  ***
Received on Friday, 16 May, 2008

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2008/0558.html
Timestamp: Saturday, 06-Feb-2016 11:35:24 PST
Retrieved: Saturday, 22-Feb-2020 07:54:06 GMT