Conservation DistList Archives [Date] [Subject] [Author] [SEARCH]

Subject: Housing brass dies

Housing brass dies

From: Ian Bogus <ian.bogus<-a>
Date: Friday, July 18, 2008
I am working a collection of brass dies used for publishers cloth
books.  They will be housed in artifact trays but am having some
difficulty deciding on what type of padding to use to keep them from
moving around.  The trays are about 1 inch high and the dies are
less than 1/4 inch.  Does anyone have experience or suggestions they
can share?

Ian Bogus
Head, Collections Care
Preservation Department
Yale University Libraries
130 Wall Street
PO Box 208240
New Haven CT 06520-8240
203-432-1721
Fax: 203-432-9900


                                  ***
                  Conservation DistList Instance 22:6
                  Distributed: Saturday, July 19, 2008
                        Message Id: cdl-22-6-024
                                  ***
Received on Friday, 18 July, 2008

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2008/0809.html
Timestamp: Saturday, 06-Feb-2016 11:35:24 PST
Retrieved: Wednesday, 16-Oct-2019 16:59:56 GMT