Ingeborg Eggink <ieggink [at] stadsarchief__amsterdam__nl> writes

>We would like to use the sandwich-method (mounting the broken pieces
>between new glass plates). I would like to know which type of glass
>can be used best for the 'sandwich' (composition, thickness etc.)

I would recommend Katharine Whitman's final report for the Advanced
Residency Program in Photograph Conservation, titled "History and
Conservation of Glass Supported Photographs", available in PDF:

    <URL:http://www.arp-geh.org//indexsep.aspx?nodeidp=401>

Katharine addresses most of the issues regarding conservation of
these objects and presents many case studies you may find useful.

Luisa Casella


                                  ***
                  Conservation DistList Instance 22:18
                Distributed: Sunday, September 28, 2008
                       Message Id: cdl-22-18-005
                                  ***
Received on Monday, 22 September, 2008

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2008/1052.html
Timestamp: Saturday, 06-Feb-2016 11:35:24 PST
Retrieved: Friday, 22-Feb-2019 21:24:55 GMT