The followingis posted on behalf of Apryl Sullivan
<apryls<-a t->mail< . >utexas< . >edu>

    I am in the process of housing costumes in a film collection
    that have fake blood on them. The fake blood is still tacky and
    sticks to the housing materials that touch it. I have tried
    polyester film, Tyvek, and also a teflon coated material. I
    would appreciate any ideas and suggestions that you might have.

    Apryl Sullivan
    Manager, Preservation Housings
    Harry Ransom Center
    The University of Texas at Austin
    PO Box 7219
    Austin, Texas 78713-7219
    512-471-8128
    apryls<-a t->mail< . >utexas< . >edu


                                  ***
                  Conservation DistList Instance 22:35
                 Distributed: Monday, December 8, 2008
                       Message Id: cdl-22-35-029
                                  ***
Received on Wednesday, 3 December, 2008

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2008/1369.html
Timestamp: Saturday, 06-Feb-2016 11:35:24 PST
Retrieved: Monday, 21-Oct-2019 20:46:07 GMT