Robert Pearce <robert.pearce [at] nottingham__ac__uk> writes

>I have recently been working on a 15th Century English binding. The
>book has Beech(?) boards that are approximately 9mm thick and one of
>the boards is broken along the grain. Although this must have
>happened quite a while ago, the boards fit together quite nicely
>with good sharp clean joins. ...

Scoth glue (hide glue) seems to be the best adhesive choice for your
case. Thermoplastic, highly re-treatable and high bonding.

Ulisses Mello
CEO, conservator-restorer, Dip.Cons., PG
Ulisses Mello Restorations
Rio de Janeiro, Brazil


                                  ***
                  Conservation DistList Instance 22:68
                   Distributed: Monday, May 18, 2009
                       Message Id: cdl-22-68-007
                                  ***
Received on Saturday, 16 May, 2009

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2009/0577.html
Timestamp: Sunday, 04-Sep-2016 12:36:52 PDT
Retrieved: Friday, 20-Jul-2018 20:22:12 GMT