Subject: Modular Cleaning Program

Modular Cleaning Program

From: Chris Stavroudis <cstavrou<-at->
Date: Wednesday, October 7, 2009
The newest version of the Modular Cleaning Program (MCP) is
available for downloading from CoOL

    <URL:http://cool.conservation-us.org/byauth/stavroudis/mcp/>

This version supports aqueous cleaning systems as well as
Carbopol-based solvent gels. It also introduces a new graphic
display for visualizing the polarity and aromaticity of solvents,
solvent mixtures, and solvent gels.

The program is built using FileMaker Pro 9, but there are runtime
versions available for both Windows and Mac computers that don't
require the user to own FileMaker.

As before, a registration number is required to unlock the database.
Previously issued registration numbers will work with the new
version. New users should email Chris Stavroudis
<cstavrou<-at->ix<.>netcom<.>com> for a registration number. The Modular
Cleaning Program is for use by professional conservators. Therefore
when requesting a registration number, please provide information
about your professional status.

The new version can also read registration information from previous
versions of the MCP. When doing so, it also offers the option of
reading in the results of previous tests recorded into the database.

Chris Stavroudis
Conservator in Private Practice
Los Angeles, CA USA


                                  ***
                  Conservation DistList Instance 23:12
                 Distributed: Tuesday, October 13, 2009
                       Message Id: cdl-23-12-001
                                  ***
Received on Wednesday, 7 October, 2009

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2009/0753.html
Timestamp: Sunday, 04-Sep-2016 12:36:52 PDT
Retrieved: Wednesday, 23-Jan-2019 20:21:53 GMT