Dale Paul Kronkright <conservator [at] okeeffemuseum__org> writes

>Johanna Lang <johanna.lang [at] gmx__de> writes
>
>>Within the project "Wax Collages: Precious Craftsmanship in Danger
>>of Extinction" at the Deutsches Hygiene Museum Dresden a test series
>>on different adhesives for wax objects is being carried. ...
>
>I suggest experiments with various mixtures of
>Poly(2-ethyl-2-oxazoline) ("Aquazol, general chemical formula:
>(C5H9NO)x ) ...
>...
>I am sorry but I am unaware of EU suppliers of these products.

In 2006 I asked for stamps of Aquazol 500, 200 and 50 in Switzerland
by

    Univar AG
    Drahtzugstrasse 18
    8032 Zurich
    +41 44 384 52 31
    Fax: +41 44 422 21 66
    reto.kunzler<-at->univareurope<.>com

They send me about 200ml of each products charge free! I use Aquazol
for the consolidation of a weak adherance painting layer (aquarelle)
on transparent paper (diploma work)

Florane Gindroz
Conservator
Library of Geneva
Promenade des Bastions
1211 Geneva 4
+41 22 418 28 07


                                  ***
                  Conservation DistList Instance 23:19
                 Distributed: Sunday, November 29, 2009
                       Message Id: cdl-23-19-009
                                  ***
Received on Tuesday, 24 November, 2009

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2009/0888.html
Timestamp: Sunday, 04-Sep-2016 12:36:52 PDT
Retrieved: Wednesday, 23-Jan-2019 19:32:30 GMT