I am a student from Camberwell College of Arts, studying an MA in
book conservation, and I am currently volunteering at the Victoria
and Albert Museum.

I am working on a book at the V&A which is made from a very stiff
bright green parchment and I am getting to the stage where I will
need to repair the spine with a new piece of parchment. We have
looked into the possibility of using other materials such as tissue
and Tyvek, but due to the nature of the repair and the stiffness of
the parchment, we have returned to parchment at the best option.

I wondered whether anyone might have any advice on dying parchment?
Or perhaps some articles that may come in handy?

I have never done it before, so I am really looking for any
information, such as what paints to use, etc.

Maudie Gunzi
+44 7743447701


                                  ***
                  Conservation DistList Instance 26:14
                 Distributed: Saturday, August 25, 2012
                       Message Id: cdl-26-14-018
                                  ***
Received on Wednesday, 22 August, 2012

[Search all CoOL documents]


URL: http://cool.conservation-us.org/byform/mailing-lists/cdl/2012/0918.html
Timestamp: Sunday, 12-Jun-2016 11:50:37 PDT
Retrieved: Sunday, 15-Dec-2019 13:32:14 GMT